409 is an 11% chromium ferritic stainless with no nickel — it handles exhaust temperatures (550-650 °C) at roughly half the price of 304, but only 304 resists chlorides, acids and food-contact duty. 304 is 18% Cr + 8% Ni, non-magnetic when annealed, and the default for kitchen, chemical and architectural work. Choose 409 for heat + cost; choose 304 for corrosion + hygiene.
Every stainless buyer crosses this decision: the cheap heat-resistant ferritic (409) or the all-round austenitic (304). They are not interchangeable — each wins a different job. Here is the comparison table we use when customers ask, followed by the decision logic.
Side by Side
| Property | 409L (1.4512) | 304 (1.4301) |
|---|---|---|
| Family | Ferritic | Austenitic |
| Chromium | 10.5–11.7% | 17.5–19.5% |
| Nickel | None | 8.0–10.5% |
| Corrosion resistance | Mild atmosphere, high temp | Wide range: acids, chlorides (moderate), food |
| Max service temp (oxidation) | 550–650 °C | ≈ 800 °C (but creep-weak above 500 °C — use 304H) |
| Magnetic | Yes (normal, not a defect) | No (annealed) |
| Price vs 304 | ≈ 50–60% | baseline (tracks nickel price) |
| Typical duty | Exhaust systems, heat shields | Kitchen, chemical, architecture, food |
The Decision Table
| If Your Part… | Order | Why |
|---|---|---|
| Carries hot exhaust gas | 409L | Mufflers, pipes, converter shells — 409 is the OEM standard: 409L guide |
| Touches food or chemicals | 304 | Hygiene + corrosion — no ferritic substitute |
| Sits outdoors near the sea | 304 (or 316) | Chlorides pit ferritics fast |
| Needs high temp and strength above 500 °C | 304H | The high-carbon 304 for boilers: 304H guide |
| Is price-sensitive and mildly corrosive | 409L | Half the price does the same job at exhaust temps |
Two Traps to Avoid
- The magnet test misleads: 409 is magnetic and buyers sometimes reject it as "not real stainless" — ferritic stainless is magnetic by metallurgy, not by quality. Judge by the MTC, not a magnet.
- Nickel price swings: 304's price tracks the LME nickel price week to week; 409 is nickel-free and much more stable to quote. Long-term programs in 409 lock pricing far better.
What We Ship
Both grades from Foshan: 409L coil/sheet/strip 0.4–6.0 mm (full 409L spec) and 304/304L/304H plate and coil 0.4–100 mm (304H for high temp, 304/304L plate sizes) — EN 10204 3.1 MTC per heat, cut-to-size and slit-to-width, MOQ 5 t. Recent shipment: 304H + 409L consolidated container to Haiphong.
Send the part — we name the grade
Application, thickness and quantity to [email protected] or WhatsApp +86 191 5745 8011 — 409L and 304 priced side by side in one quotation. MOQ 5 t.
Request Stainless Quote