EN 10219 hollow sections are cold-formed from strip and seam-welded β cheaper, tighter corners, wider size range; EN 10210 sections are hot-finished β better toughness (impact values guaranteed), larger corner radii, preferred for fatigue and low-temperature service. Both carry S235/S275/S355 (+J2H/K2H classes for 10210). Chinese mills supply both, MOQ 5 t.
Two EN standards, same-looking tube, different metallurgy. Buyers of structural hollow sections (SHS/RHS/CHS) choose between them β and the choice matters most for cold climates, fatigue and heavily welded joints.
The Core Differences
| EN 10219 (cold-formed) | EN 10210 (hot-finished) | |
|---|---|---|
| Process | Strip roll-formed and seam-welded at room temperature | Formed hot from billet or strip at forming temperature |
| Corner radii | Tight (β€ 1.5β2.5 t) | Larger (β 1.0β1.5 t, softened) |
| Toughness | Standard grades (J2H available per part) | Guaranteed impact values (K2H etc.) β better for cold service |
| Residual stress | Higher (cold work) | Lower (hot work relieves) |
| Size range | Wider (wall thinner relative to section) | More limited |
| Price | Lower | +10β25% |
| Order For | General structures, weldable frames, moderate climates | Corrosive/cold environments, fatigue, heavy welded nodes |
Grades in Each Standard
| EN 10219 | EN 10210 | Yield (β€16 mm) |
|---|---|---|
| S235RH / S275J0H / S355J2H | S235JRH / S275J0H / S355K2H | 235 / 275 / 355 MPa |
| S460MH | S460NH | 460 MPa (high-strength options) |
The H suffix marks hollow-section grades with tighter impact and sulfur limits than flat-product twins.
Decision Rules
- Indoor frames, moderate climate, cost-driven β 10219 cold-formed (the volume choice).
- Offshore/coastal, β20 Β°C service, crane or fatigue nodes β 10210 hot-finished with guaranteed impact.
- Heavy welded nodes without preheat β 10210 (lower residual stress and corner hardness).
- US-spec equivalents: cold-formed per A500; hot-finished has no exact US twin.
Supply from China
- Both standards: square 20Γ20β400Γ400, rectangular to 100Γ400, round to DN200: size table Β· A500 comparison
- Grades S235/S275/S355 (+J2H/K2H), 3.1 MTC per heat.
- MOQ 5 t; mixed 10219+10210 in one container allowed.